tech / sci.engr.joining.welding / Re: Ali GMAW - defect rates - spray, pulse

SubjectAuthor
* Ali GMAW - defect rates - spray, pulseRichard Smith
`- Ali GMAW - defect rates - spray, pulseRichard Smith

1
Ali GMAW - defect rates - spray, pulse

<ly1qt3v3so.fsf@void.com>

  copy mid

http://rslight.i2p/tech/article-flat.php?id=806&group=sci.engr.joining.welding#806

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!aioe.org!bsCryoC9F9xusoDHIbn6tw.user.46.165.242.91.POSTED!not-for-mail
From: null@void.com (Richard Smith)
Newsgroups: sci.engr.joining.welding
Subject: Ali GMAW - defect rates - spray, pulse
Date: Fri, 26 Aug 2022 08:53:43 +0100
Organization: Aioe.org NNTP Server
Message-ID: <ly1qt3v3so.fsf@void.com>
Mime-Version: 1.0
Content-Type: text/plain; charset=us-ascii
Injection-Info: gioia.aioe.org; logging-data="35047"; posting-host="bsCryoC9F9xusoDHIbn6tw.user.gioia.aioe.org"; mail-complaints-to="abuse@aioe.org";
User-Agent: Gnus/5.11 (Gnus v5.11) Emacs/22.1 (darwin)
Cancel-Lock: sha1:kxc2a2m6I6+AXA73pLS7mQL1M5Y=
X-Notice: Filtered by postfilter v. 0.9.2
 by: Richard Smith - Fri, 26 Aug 2022 07:53 UTC

Hi
Plea for real experience information.
Thicker Ali at above about 130A.
Probably wire-feed-speed at or above 10m/min (394ipm)
Thinking of marine-grade 5000-series Al-Mg, but experience of other
grades would apply regarding this question.
For welds, compare / contrast:

* spray-transfer/smooth-run
^
v
* Pulse-mode/stepped-progression

Or any comparison of spray/Pulse modes and of smooth/stepping
progression.

Flaw and defect rates, please.
This would be by radiography (x-ray) and mechanical test (strength
alone will reveal everything important about Ali?).

Here in UK we have an orthodoxy about which process / approach must be
used.
Defect rates are / can-be high.
Which surely simply cannot be the case universally???
Unfortunately I have not been able to test the welds I trust the most.

Thanks in advance,
Rich Smith

Re: Ali GMAW - defect rates - spray, pulse

<lya67r3vsg.fsf@void.com>

  copy mid

http://rslight.i2p/tech/article-flat.php?id=811&group=sci.engr.joining.welding#811

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!aioe.org!XT8ZdeRI7rN/pu9rRN1H6w.user.46.165.242.91.POSTED!not-for-mail
From: null@void.com (Richard Smith)
Newsgroups: sci.engr.joining.welding
Subject: Re: Ali GMAW - defect rates - spray, pulse
Date: Fri, 26 Aug 2022 15:48:47 +0100
Organization: Aioe.org NNTP Server
Message-ID: <lya67r3vsg.fsf@void.com>
References: <ly1qt3v3so.fsf@void.com>
Mime-Version: 1.0
Content-Type: text/plain; charset=us-ascii
Injection-Info: gioia.aioe.org; logging-data="5170"; posting-host="XT8ZdeRI7rN/pu9rRN1H6w.user.gioia.aioe.org"; mail-complaints-to="abuse@aioe.org";
User-Agent: Gnus/5.11 (Gnus v5.11) Emacs/22.1 (darwin)
X-Notice: Filtered by postfilter v. 0.9.2
Cancel-Lock: sha1:ByMqwBFKzAU0UnSG0iTJuLeorFs=
 by: Richard Smith - Fri, 26 Aug 2022 14:48 UTC

10m/min - that's with 1.2mm wire...